The total coating thickness is above 1.5mm, and the coating interval is 2-12h (depending on the weather condition). 1-2 layers of glass fiber cloth or other matrix material can be added to the coating.
Coating: construction can be used to roll, scrape, paint and brush can be, generally painted 3-4 scraping, each scraping scraping reference amount of 0.8-1.0 kg / square meter.
Seam treatment: if the roof has more than 3mm cracks, sealing materials should be filled, and then coated with scraping coating.
Basic level treatment: the surface of the base layer is required to be smooth, and uneven sand lifting is not allowed.