Answer:

Increase the refractoriness and looseness of core sand
If is casting, internal shell mold may be not completely dry, strength is not enough, resulting in shell mold collapse into molten steel.It is also possible that the refractory is not refractory enough.
Valve sand core mold drying is not in place, excessive water content