Home > categories > Minerals & Metallurgy > Binder > Adhesive viscosity is not enough, and is not related to acidity?
Question:

Adhesive viscosity is not enough, and is not related to acidity?

Adhesive viscosity is not enough, and is not related to acidity?

Answer:

Terms of settlement1, add oxidant, continue to respond2, increase the temperature of the reaction fluid3, prolong oxidation gelatinization time (summer reaction is stable 2 hours to 3 hours, winter is best to stabilize one night)The binder reacted with caustic soda for 40 minutes to 60 minutes, and the viscosity was too low
Reason1, oxidant dosage is insufficient or content is low2, the oxidation reaction temperature is low3, short oxidation time
Not alwaysIt has a lot to do with temperature and timeThe binder reacted with caustic soda for a certain period of time and the viscosity was too high