Home > categories > Minerals & Metallurgy > Aluminum Bars > Aluminum rods are always black after homogenization, how to deal with 30T gas homogeneous furnace?
Question:

Aluminum rods are always black after homogenization, how to deal with 30T gas homogeneous furnace?

Aluminum rods are always black after homogenization, how to deal with 30T gas homogeneous furnace?

Answer:

2, the incomplete combustion of natural gas burner, check the burner flame inside normal combustion state, then it should be blue point.
1, cast bar surface oil, check the cast well, there is no oil leakage inside what?.
1, cast bar surface oil, check the cast well, there is no oil leakage inside what?.2, the incomplete combustion of natural gas burner, check the burner flame inside normal combustion state, then it should be blue point.