Glass fiber reinforced plastic GRE pipe broken hole how to repair and repair?
Resin selection of good points, the general also line, as well as accelerators, curing agents, high-quality glass fiber cloth.
Don't let the powder go. It is autumn, the temperature is low, so to put more than summer curing agent, as to the exact proportion, I just guess should be: curing agent, accelerator, resin; 1:1.5:8 with glass fiber wrapped around the pipe, coated on the glass fiber cloth to make glass steel with good quickly, let the glass steel the glass fiber cloth fully soaked, waiting for the full glass steel after curing, and then repeated several layers. It will be strong.