Question:

How to cast aluminum parts

How to cast aluminum parts

Answer:

After the molten aluminum, the temperature increased to more than 850 degrees, adding silicon powder mixing, heat preservation 40-60min, the temperature of 720-750 degrees into the metal mold can be.
It's simple. First put the aluminum into the graphite crucible, and the equipment is preferably a medium frequency induction furnace.