I would like to have a one meter high body sculpture turned into glass fiber reinforced plastic, please ask how thick coated resin, glass fiber cloth should be paved several layers of solid?There is a first mold coating resin coating, or the first in each block die inside coating to be dry and mold, is the first time I turned the glass steel
The wall thickness of 3mm resin on the line, as long as a layer of glass cloth can be, if you want to use the gel coat resin, resin glass steel production when first brushes in the mold inside the gel with good. Each piece of mold in the resin brush, glass cloth affixed to all the solidification of the scraping edge of the mold. Repair after demoulding.
Even if I told you the way! And you'll mess it up! No, try it!
In order to make the surface coating can be perfect every time the best coating brush to ensure uniform is best not to paint too good again after curing second timethen brushing to second gel cured thick fiber cloth with ordinary polyester resin paste a layer 0.2 of the fine fiber cloth layer 0.4 to two are not fully the cured blade edge and then repaired with wallpaper on the OK mode