Iron type frequency furnace, billet 150, continuous casting billet between the hole, please help net friend to find the original, please ask non answer, not Xie, please mention, understand enough, please resume me

Answer:

1: new furnace, new furnace lining contains more gas2: raw material no clean, no coincidence?3: melt protection? Temperature is not high, no refining and static?4:3 point, mold and traction to look for defects, mold cooling effect - water temperature - traction line and horizontal - traction process5: stop and pull
Production: 1 steel and 2 steel alloy or damp; for ladle lining refractory and no baking; otherwise the whole section are 3 billet bubble deposit if the situation is steel quality problems and the main problems of alloy billet; if the bubble is mainly between now and the relationship between process equipment (including continuous casting are clearly some problems of continuous casting machine the parameters of a)