What is the iron loss value of 50W250 silicon steel sheet?
This brand is produced very little, 0.5 of the thickness of the best is 270, the market is more common. 250 basically the thickness of the 0.35MM.
The theoretical iron loss value is 2.5., and Baosteel is estimated to be around 2.2. TISCO can reach the level of 2.18-2.25, which is little different from that of wisco. (P15/50 B50 W/kg), imports of Japan's relatively good material, can reach about 2.12.