Ductile iron 600-3 grade, tensile strength, how to test, there is a simple way?

Ductile iron 600-3 grade, tensile strength, how to test, there is a simple way?

Answer:

General use of tensile machines, such as quality management, this aspect should be strictly controlled, otherwise the data is not accurate, do nothing, no one wants
Generally use tensile machine to do, I often operate, or you see the metallographic 3J above perlite 60% above should be no problem
600-3 is pearlite + a small amount of ferrite matrix ductile iron. Pearlite edge region. 10%, center. 70600-3. Two sets of numbers indicating the grades and mechanical properties of nodular cast iron. The former represents the minimum tensile strength