Insulation brick should pay attention to external walls?
Using special powder pointing pointing, check the horizontal joints and then hook the vertical slot, after cancelling the recessed brick outer surface 2mm, tile seam after hook silk or cotton cloth clean, after inspection of the large area pointing outside the walls, should be the implementation of a large area of local cleaning after cleaning, to ensure the whole project clean and beautiful.
Construction at room temperature, 24h after spraying water conservation, water spraying should not be too much, not flow. Unsuitable for winter construction. According to the national standard, seven consecutive days and nights, the average temperature is less than 5 degrees, may not carry on the external wall insulation, brick construction.
In each segment or block the tiles are from bottom to top paste, from the line of position the next layer of hypodermis first brick hidden good ruler, to hold the first leather tiles, pull in tile lines as the upper skin paste standard.
Before the tile is adhered, the water spraying device is applied to spray the wet water on the adhered base layer so as not to flow better.