Some of the copper clad tiles are roughened. Why not some of them? What are the factors?
When the filler is added with or without padding, the TG will generally rise and the plate will be stiffer;
2. press the thermostat temperature, CCL is generally set at 200 degrees or more, the higher the TG, the higher the set temperature;
Press dwell time length, CCL is generally set above 60min, the higher the TG, the longer the set time;
The resin type is the determining factor. This is the CCL plant knowhow and is generally not released.