Why the temporary building interior lime mortar plaster, a period of time after the wall generally cracked?
The key is the material and the construction process, the sand is too thin or mud is too large, lime ripening is not good. Construction technology is not in place, mortar with the amount of lime is too large, plastering the wall before the end of the water is not uniform, plastering rubbing ram is not in place, lime cream when the surface is not uneven thickness, no second survival and so will cause cracking , So you have to analyze the reasons for the actual situation according to the scene.
Why the temporary building interior lime mortar plaster, a period of time after the wall generally cracked?