Home > categories > Construction & Real Estate > Veneers > Brief description of veneer production process
Question:

Brief description of veneer production process

Brief description of veneer production process

Answer:

Of the wooden side should be promptly placed in the paver before the wood temperature of the tank, the insulation in the range of 40 ~ 50 ℃ (with the species and thin wood thickness may be).
so as to avoid the thermal stress caused by wood cracking. The cooking pool should often clear the resin, bark, sediment, and often change the water, to reduce the pollution of the wood
First, the wooden side into the cooking pool, the tree species, wooden specifications should be carried out separately; water temperature is best to maintain room temperature, and slowly warming,
; after cooking treatment; the cooking process should be reduced to more than 40 ℃, it should slow down the heating rate