How to improve the quality of nodular cast iron pipe fittings
For cast iron pipe chute taphole bent or improper chute taphole distance socket distance, easy to form a skin defect in cast iron pipe socket parts, equipment manufacturing inspection of cast iron pipe fittings must be in production, replacing the cast iron pipe chute taphole elbow when necessary, and adjust the host making iron centrifuge when the pipe in the lower limit, shorten the chute taphole socket from the distance.
To avoid the iron pipe inner wall of mold management lean reduce iron pipe pipe mould run speed, can make a dense and uniform pitting; avoid mold wall cast iron pipe pipe packed too shallow, increase the pressure, wear a good play to nod, can ensure the suitable depth of pitting.For pipes with grease and debris on the inner surface, especially the new cast iron pipe fittings, the grease and sundries on the surface of the cast iron pipe can be removed before use. For the cast iron pipe mould with a crack of a turtle, it is slight to use. When in use, the amount of mould powder should be increased; if the crack of the turtle is serious, the cast iron pipe mould must be replaced in time.
When the molten iron temperature is too low and the inner wall temperature of the tube is low, heavy skin defects will occur. When the molten iron temperature is high and the molten iron gas increases, porosity defects can be generated. In the medium frequency furnace, the hot metal should be provided according to the process specification, and the temperature of the inlet and outlet and the cooling rate can be controlled reasonably in the process of production.