Suction flat test: in the 1min vacuum, after maintaining 10min, with diameter of 0.9 times the diameter of the hose rolled over, check the degree of collapse of the hose. Some standards used to measure the rate of change in the outer diameter of the hose to indicate the extent of deformation of the hose.
Bending test: after bending the hose to a certain extent, measure the minimum outside diameter of the bending part and the ratio of the outside diameter before bending, the passing capacity of the steel ball and the bending force when the tube is pressurized.
Low temperature bending test at low temperature: hose clamp on rigid torsion wheel diameter hose diameter 12 times, for 6 hours at a low temperature, twisted 180 degrees within 12s when the measured torque and the standard temperature measured torque ratio. Low temperature bending: hose clamped in the diameter of the hose within 12 times the torsion wheel, parked at low temperatures for 24 hours, in the 10s to reverse 180 degrees, check whether or not the internal and external plastic brittle fracture and damage.
Hydraulic test verification pressure test: Test hose and assembly under verification pressure, continue 30s-60s, whether to produce leakage, deformation and damage. Compression deformation test: keep 1 minutes under the specified pressure (work pressure, verification pressure or other pressure below the proof pressure), measure the length and diameter of the hose, twist angle and bend. Bursting pressure test: Determination of the pressure at which the hose burst during the specified step-up rate.
Hose size measurement: the inner and outer diameter, outer diameter, wall thickness, enhancement layer concentricity, inner and outer layer of glue thickness, assembly diameter, new GB and ISO increased the length and the measuring point mark, provides no pipe joint and a hose length of various pipe joint measurement method.