There is also the best welding, gas welding and local heating to 400 degrees, direct flame heating for about 3 minutes, and then covered with wood powder, so that solder hardness and parent material almost, then YT5 will be turning!
Otherwise, none of the knives will work! There is also the best welding, gas welding and local heating to 400 degrees, direct flame heating for about 3 minutes, and then covered with wood powder, so that solder hardness and parent material almost, then YT5 will be turning!
YT5 is better! However, if the surface of cast steel sand hole, or sand lot, recommended to use gas welding and other heating tool on the surface is heated to 60 degrees Celsius, in the processing, multiplier!